This section is from the book "A Practical Workshop Companion For Tin, Sheet Iron, And Copper Plate Workers", by Leroy J. Blinn. Also available from Amazon: A Practical Workshop Companion For Tin, Sheet Iron, And Copper Plate Workers.

Size. | Diam. of top. | Diam. of bot. | Height. | ||||
5 | gal. | 8 | in | 13 1/2 | in | 12 3/8 | in |
3 | " | 7 | 11 1/2 | 10 1/8 | |||
2 | " | 6 | 10 1/2 | 8 3/8 | |||
1 | " | 3 3/4 | 8 3/4 | 7 1/2 | |||
Size. | Diam. of top. | Diam. of bot. | Height | ||||
1/2 | gal. | 3 1/8 | in | 6 5/8 | in | 6 | in |
1 | qt. | 2 1/2 | 5 1/8 | 4 7/8 | |||
1 | pt. | 2 | 4 | 4 | |||
1/2 | " | 1 3/4 | 3 3/4 | 3 1/8 | |||
American Lap Weled Iron Boiler Flues, Manufactured by the Reading Iron Company.
Outside Diameter. | W. G. Nos. | Weight per Foot, about, |
1 1/4 in. | 16 | 1 lb. |
1 1/2 | 15 | 1 1-10 |
1 3/4 | 14 | 1 1/2 |
2 | 13 | 2 |
2 1/4 | 12 | 2 1/2 |
2 1/2 | 12 | 2 3/4 |
2 3/4 | 11 | 3 1/3 |
3 | 11 | 3 1/2 |
Outside Diameter, | W, G, Nos: | Weight per Foot, about |
3 1/4 | 11 | 4 |
3 1/2 | 10 | 4 3/4 |
4 | 10 | 5 1/2 |
5 | 9 | 7 1/2 |
6 | 8 | 10 |
7 | 7 | 13 |
8 | 6 |
Table of Effects upon Bodies by Heat.
FAHRENHEIT. | ||
Cast Iron thoroughly smelts at................... | 2754° | |
Fine Gold melts | ,, ............................ | 1983° |
Fine Silver melts | ,, ............................ | 1850° |
Copper melts | ,, ............................ | 2160° |
Brass melts | ,, ............................ | 1900° |
Zinc melts | ,, ............................ | 740o |
Lead melts | ,, ............................ | 594o |
Bismuth melts | ,, ............................ | 476° |
Tin melts | ,, ............................ | 421° |
Tin and Bismuth equal parts melt........................ | 283o | |
Tin 3 parts Bismuth 5 and Lead 2 melt........................ | 212o | |
 
Continue to: