When fine (No. 1,) or super-carbonated crude iron is run from the furnace, the stream of metal, as it issues from the fauld, throws off an infinite number of brilliant sparkles of carbon. The surface is covered with a fluid pellicle of carburet of iron, which, as it flows, rears itself up in the most delicate folds; at first the fluid metal appears like a dense ponderous stream, but as the collateral moulds become filled, it exhibits a general rapid motion, from the surface of the pigs to the centre of many points. Millions of the finest undulations move upon each mould, displaying the greatest nicety and rapidity of movement, conjoined with an uncommonly beautiful variegation of colour, which language is inadequate justly to describe. Such metal, in quantity, will remain fluid for twenty minutes after it has run from the furnace, and, when cold, will have its surface covered with beautiful carburet of iron, already mentioned, of an uncommonly rich and beautiful appearance. When the surface of the metal is not carburetted, it is smooth, like forged iron, and always convex.

In this state iron is too rich for melting without the addition of coarse metal, and is unfit to be used in a cupola furnace for making fine castings, where thinness and a good skin are requisite.

No. 4, or oxygenated crude iron, when issuing from the blast furnace, throws oft from all parts of the fluid surface a vast number of metallic sparks, and, while running, it is covered with waving flakes of an obscure smoky flame, accompanied with a hissing noise. This is a slight sketch of the appearances of the two extreme qualities of crude iron, when in a state of fusion. There still remain two intermediate stages of quality to be described; these are, carbonated, and carbo-oxygenated iron, that is, No. 2 and No. 3 of the manufacturers.

No. 2, or carbonated iron, exhibits, like No. 1, a beautiful appearance in the runner and pig. The breakings of the fluid, in general, are less fine, the agitation less delicate, though the division of the fluid is equal, if not beyond, that of the other.

No. 3, or carbo-oxygenated iron, runs smoothly, without any great degree of ebullition, or disengagement of metallic sparks. The partings upon its surface are longer, and at greater distances from each other than in the former varieties; the shape they assume is either elliptical, circular, or curved. In cooling, this metal acquires a considerable portion of oxide. An infallible criterion of the quality of the iron in the furnace is afforded by the colour of the scoriae upon the working bars, which are from time to time inserted to keep the furnace free from lumps, and to bring forward the scoriae. When No. 1, or super-carbonated iron, is on the hearth, the vitriol crust upon the bars will be of a black colour and smooth surface, fully covered with large and brilliant plates of plumbago. As the quality of the metal approaches to No. 2, (carbonated,) the carburet upon the scoriae decreases both in point of quantity and size. When carbo-oxygenated (No. 3) is in the furnace, the working bars are always coated with a lighter coloured scoriae than when the former varieties exist; a speck of plumbago is now only found here and there; and when the quality of the metal is oxygenated (No 4), not only have the plates of carburet disappeared, but also the crally colour on the external surface of the scoriae.

It may perhaps be proper here to mention, that although for convenience the manufacturer has, from a just estimation of the value of the metal in a subsequent manufacture, affixed certain numbers for determinate qualities of iron, yet it is difficult to say at what degree of saturation of carbon each respective term commences; suffice it then to say, that the two alterative principles, oxygen and carbon, form two distinct classes - that in which oxygen predominates, and that in which carbon predominates.